Comparison of the fracture strengths of metal-ceramic crowns and three ceromer crowns

To access this article, please choose from the options below

Login to an existing account or Register a new account.

  • Purchase this article for 15.00 USD (You must login/register to purchase this article)

    Online access for 24 hours. The PDF version can be downloaded as your permanent record.

  • Subscribe to this title

    Get unlimited online access to this article and all other articles in this title 24/7 for one year.

  • Claim access now

    For current subscribers with Society Membership or Account Number.

  • Visit SciVerse ScienceDirect to see if you have access via your institution.

 Reprint requests to: Dr Hong-So Yang, Department of Prosthodontics, College of Dentistry, Chonnam National University, Hak-Dong 8, Dong-Ku, Kwang-ju 501-191, KOREA, Fax: (82)62-227-7426, E-mail: yhsdent@chonnam.ac.kr

☆☆ aResident, Department of Prosthodontics.

 bAssistant Professor, Department of Prosthodontics.

★★ cProfessor and Chairman, Department of Prosthodontics.

PII: S0022-3913(02)00074-4

doi: 10.1067/mpr.2002.127712

Journal of Prosthetic Dentistry
Volume 88, Issue 2 , Pages 170-175 , August 2002