« Previous
Next »
Journal of Prosthetic Dentistry
Volume 88, Issue 4
, Pages 388-395
, October 2002
Marginal accuracy and fracture strength of ceromer/fiber-reinforced composite crowns: Effect of variations in preparation design
References
- . Flexural properties of acrylic resin polymers reinforced with unidirectional and woven glass fibers. J Prosthet Dent. 1999;81:318–326
- . Development and clinical applications of a light-polymerized fiber-reinforced composite. J Prosthet Dent. 1998;80:311–318
- . The reinforcement of dentures. J Oral Rehabil. 1999;26:185–194
- . In-vitro study of fracture strength and marginal adaption of fibre-reinforced adhesive fixed partial inlay dentures. J Dent. 1999;27:163–168
-
.
In vitro study of fracture strength and marginal adaptation of fibre-reinforced-composite versus all ceramic fixed partial dentures.
Eur J Prosthodont Rest Dent. 1998;6:55–62
- . Clinical and scanning electron microscopic evaluation of fiber-reinforced inlay fixed partial dentures: preliminary results after one year. J Prosthet Dent. 1999;82:662–668
- . Epoxy/carbon composite resins in dentistry: mechanical properties related to fiber reinforcements. J Prosthet Dent. 1994;72:245–249
-
.
Adhesive crowns and fixed partial dentures fabricated of ceromer/FRC: clinical and laboratory procedures.
Pract Periodontics Aesthet Dent. 1998;10:487–498
- . Second generation laboratory composite resin for indirect restorations. J Esthet Dent. 1997;9:108–118
-
.
Aesthetic guidelines for second-generation indirect inlay and onlay composite restorations.
Pract Periodontics Aesthet Dent. 1998;10:423–431
-
.
Adhesive crowns and fixed partial dentures of optimized composite resin with glass fiber-bonded framework.
Quint Dent Tec. 1999;107–127
- . Evaluation of the marginal accuracy of different all-ceramic crown systems after simulation in the artificial mouth. J Oral Rehabil. 1999;26:582–593
- . Microleakage—full crowns and the dental pulp. J Endod. 1992;18:473–475
- . A comparison of the marginal fit of In-Ceram, IPS Empress, and Procera crowns. Int J Prosthodont. 1997;10:478–484
- . Marginal accuracy and fracture strength of conventional and copy-milled all-ceramic crowns. Int J Prosthodont. 1995;8:303–310
- . Seating accuracy and fracture strength of vented and nonvented ceramic crowns luted with three cements. J Prosthet Dent. 1995;74:18–24
- . Marginal fit of restorations before and after cementation in vivo. Int J Prosthodont. 1993;6:585–591
- . Precision of fit: the Procera AllCeram crown. J Prosthet Dent. 1998;80:394–404
- . Fracture strength of all-ceramic crowns. Int J Prosthodont. 1994;7:329–338
- . The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli. Int J Prosthodont. 1993;6:462–467
- . Dental luting agents: A review of the current literature. J Prosthet Dent. 1998;80:280–301
- . Influence of glass-ceramic thickness on Hertzian and bulk fracture mechanisms. Int J Prosthodont. 1998;11:27–32
-
.
Fracture strength of the IPS Empress crown: the effect of occlusal depth and axial inclination on upper first premolar crowns.
J Kor Acad Prosthodont. 1999;37:127–133
- . A comparative strength study of metal ceramic and all-ceramic esthetic materials: modulus of rupture. J Prosthet Dent. 1989;62:476–479
- . Effect of convergence angle on retention of resin-bonded retainers cemented with resinous cements. J Prosthet Dent. 1997;77:475–481
-
.
Restorative dental materials.
In: 10th ed. St Louis: : Mosby; 1996;p. 56
- . Fracture strength of full-contoured ceramic crowns and porcelain-veneered crowns of ceramic copings. J Prosthet Dent. 1994;71:462–467
- . Fracture-surface analysis of dental ceramics. J Prosthet Dent. 1989;62:536–541
- . Stress analysis of cemented or resin-bonded loaded porcelain inlays. Dent Mater. 1991;7:21–24
- . The effect of tooth preparation design on the breaking strength of Dicor crowns: 2. Int J Prosthodont. 1990;3:241–248
- . The effect of tooth preparation design on the breaking strength of Dicor crowns: 3. Int J Prosthodont. 1990;3:327–340
- . Cementation of vented crowns with low deformation. Aust Dent J. 1996;41:28–32
- . Determination of the minimum number of marginal gap measurements required for practical in-vitro testing. J Prosthet Dent. 2000;83:40–49
- . Laboratory assessment of impression accuracy by clinical simulation. J Dent. 1992;20:108–114
-
.
Handbook of orthodontics.
4th ed. Chicago: : Moyers Year Book Medical Publishers, Inc; 1988;
-
.
Marginal fidelity and fracture strength of In-Ceram crowns according to various resin cement.
J Kor Acad Prosthodont. 1998;36:888–899
-
.
Primer of bio-statistics.
4th ed. New York: : McGraw-Hill Co; 1997;
- . A comparison of the marginal fit of In-Ceram, IPS Empress, and Procera crowns. Int J Prosthodont. 1997;10:478–484
☆ Reprint requests to: Dr Seong-Joo Heo, Department of Prosthodontics, College of Dentistry, Seoul National University, 28 Youngun-Dong, Chongno-gu, Seoul 110-749, KOREA, Fax: 82-2-765-2536, E-mail: heosj@plaza.snu.ac.kr
☆☆ aAssistant Professor, Department of Prosthodontics, College of Dentistry, Kangnung National University.
★ bDoctoral student, Department of Prosthodontics, College of Dentistry, Kangnung National University.
★★ cAssistant Professor, Department of Prosthodontics and Dental Research Institute, College of Dentistry, Seoul National University.
♢ dAssociate Professor, Department of Prosthodontics and Dental Research Institute, College of Dentistry, Seoul National University.
PII: S0022-3913(02)00230-5
doi: 10.1067/mpr.2002.128378
© 2002 Editorial Council of The Journal of Prosthetic Dentistry. Published by Elsevier Inc. All rights reserved.
« Previous
Next »
Journal of Prosthetic Dentistry
Volume 88, Issue 4
, Pages 388-395
, October 2002