Journal of Prosthetic Dentistry
Volume 89, Issue 3 , Pages 268-274 , March 2003

Resin-ceramic bonding: A review of the literature

References 

  1. Cho GC, Donovan TE, Chee WW. Clinical experiences with bonded porcelain laminate veneers. J Calif Dent Assoc. 1998;26:121–127
  2. Dumfahrt H, Schaffer H. Porcelain laminate veneers. A retrospective evaluation after 1 to 10 years of service: Part II—clinical results. Int J Prosthodont. 2000;13:9–18
  3. Friedman MJ. Ask the experts: porcelain veneers. J Esthet Restor Dent. 2001;13:86–87
  4. Fradeani M. Six-year follow-up with Empress veneers. Int J Periodontics Restorative Dent. 1998;18:216–225
  5. Peumans M, Van Meerbeek B, Lambrechts P, Vanherle G. Porcelain veneers: a review of the literature. J Dent. 2000;28:163–177
  6. Blatz MB. Long-term clinical success of all-ceramic posterior restorations. Quintessence Int. 2002;33:415–426
  7. Felden A, Schmalz G, Federlin M, Hiller KA. Retrospective clinical investigation and survival analysis on ceramic inlays and partial ceramic crowns: results up to 7 years. Clin Oral Investig. 1998;2:161–167
  8. van Dijken JW, Hoglund-Aberg C, Olofsson AL. Fired ceramic inlays: a 6-year follow up. J Dent. 1998;26:219–225
  9. Hayashi M, Tsuchitani Y, Miura M, Takeshige F, Ebisu S. 6-year clinical evaluation of fired ceramic inlays. Oper Dent. 1998;23:318–326
  10. Fuzzi M, Rappelli G. Ceramic inlays: clinical assessment and survival rate. J Adhesive Dent. 1999;1:71–79
  11. Roulet JF. Longevity of glass ceramic inlays and amalgam—results up to 6 years. Clin Oral Invest. 1997;1:40–46
  12. Mormann W, Krejci I. Computer-designed inlays after 5 years in situ: clinical performance and scanning electron microscopic evaluation. Quintessence Int. 1992;23:109–115
  13. Pallesen U. Clinical evaluation of CAD/CAM ceramic restorations: 6-year report. In:  Mormann WH editors. CAD/CIM in aesthetic dentistry: CEREC 10 year anniversary symposium. Berlin: Quintessence; 1996;p. 241–253
  14. Berg NG, Derand T. A 5-year evaluation of ceramic inlays (CEREC). Swed Dent J. 1997;21:121–127
  15. Sjogren G, Molin M, van Dijken JW. A 5-year clinical evaluation of ceramic inlays (Cerec) cemented with a dual-cured or chemically cured resin composite luting agent. Acta Odontol Scand. 1998;56:263–267
  16. el-Mowafy O, Rubo MH. Resin-bonded fixed partial dentures—a literature review with presentation of a novel approach. Int J Prosthodont. 2000;13:460–467
  17. Corrente G, Vergnano L, Re S, Cardaropoli D, Abundo R. Resin-bonded fixed partial dentures and splints in periodontally compromised patients: a 10-year follow-up. Int J Periodontics Restorative Dent. 2000;20:628–636
  18. Behr M, Leibrock A, Stich W, Rammelsberg P, Rosentritt M, Handel G. Adhesive-fixed partial dentures in anterior and posterior areas: results of an on-going prospective study begun in 1985. Clin Oral Investig. 1998;2:31–35
  19. Kern M, Strub JR. Bonding to alumina ceramic in restorative dentistry: clinical results over up to 5 years. J Dent. 1998;26:245–249
  20. Malament KA, Socransky SS. Survival of Dicor glass-ceramic dental restorations over 14 years: Part I. Survival of Dicor complete coverage restorations and effect of internal surface acid etching, tooth position, gender, and age. J Prosthet Dent. 1999;81:23–32
  21. Malament KA, Socransky SS. Survival of Dicor glass-ceramic dental restorations over 14 years. Part II: effect of thickness of Dicor material and design of tooth preparation. J Prosthet Dent. 1999;81:662–667
  22. Malament KA, Socransky SS. Survival of Dicor glass-ceramic dental restorations over 16 years. Part III: effect of luting agent and tooth or tooth-substitute core structure. J Prosthet Dent. 2001;86:511–519
  23. el-Mowafy O. The use of resin cements in restorative dentistry to overcome retention problems. J Can Dent Assoc. 2001;67:97–102
  24. Sorensen JA, Kang SK, Avera SP. Porcelain-composite interface microleakage with various porcelain surface treatments. Dent Mat. 1991;7:118–123
  25. Reference deleted.
  26. Jensen ME, Sheth JJ, Tolliver D. Etched-porcelain resin-bonded full-veneer crowns: in vitro fracture resistance. Compendium. 1989;10:336–338 340-1, 344-7
  27. Fradeani M. Anterior maxillary aesthetics utilizing all-ceramic restorations. Pract Periodontics Aesthet Dent. 1995;7:53–66
  28. Touati B, Quintas AF. Aesthetic and adhesive cementation for contemporary porcelain crowns. Pract Proced Aesthet Dent. 2001;13:611–620
  29. Latta MA, Barkmeier WW. Approaches for intraoral repair of ceramic restorations. Compend Contin Educ Dent. 2000;21:635–639 642-4
  30. Semmelmann JO, Kulp PR. Silane bonding porcelain teeth to acrylic. J Am Dent Assoc. 1968;76:69–73
  31. Jochen DG, Caputo AA. Composite resin repair of porcelain denture teeth. J Prosthet Dent. 1977;38:673–679
  32. Ferrando JM, Graser GN, Tallents RH, Jarvis RH. Tensile strength and microleakage of porcelain repair materials. J Prosthet Dent. 1983;50:44–50
  33. Bailey LF, Bennet RJ. DICOR surface treatments for enhanced bonding. J Dent Res. 1988;67:925–931
  34. Wolf DM, Powers JM, O'Keefe KL. Bond strength of composite to porcelain treated with new porcelain repair agents. Dent Mater. 1992;8:158–161
  35. Sorensen JA, Engelman MJ, Torres TJ, Avera SP. Shear bond strength of composite resin to porcelain. Int J Prosthodont. 1991;4:17–23
  36. Chen JH, Matsumura H, Atsuta M. Effect of different etching periods on the bond strength of a composite resin to a machinable porcelain. J Dent. 1998;26:53–58
  37. Chen JH, Matsumura H, Atsuta M. Effect of etchant, etching period, and silane priming on bond strength to porcelain of composite resin. Oper Dent. 1998;23:250–257
  38. Barghi N. To silanate or not to silanate: making a clinical decision. Compend Contin Educ Dent. 2000;21:659–662 664
  39. Kamada K, Yoshida K, Atsuta M. Effect of ceramic surface treatments on the bond of four resin luting agents to a ceramic material. J Prosthet Dent. 1998;79:508–513
  40. Estafan D, Dussetschleger F, Estafan A, Jia W. Effect of prebonding procedures on shear bond strength of resin composite to pressable ceramic. Gen Dent. 2000;48:412–416
  41. Della Bona A, Anusavice KJ, Shen C. Microtensile strength of composite bonded to hot-pressed ceramics. J Adhes Dent. 2000;2:305–313
  42. Rosentritt M, Behr M, Kolbeck C, Lang R, Handel G. In vitro repair of all-ceramic and fibre-reinforced composite crowns. Eur J Prosthodont Restor Dent. 2000;8:107–112
  43. Kupiec KA, Wuertz KM, Barkmeier WW, Wilwerding TM. Evaluation of porcelain surface treatments and agents for composite-to-porcelain repair. J Prosthet Dent. 1996;76:119–124
  44. Thurmond JW, Barkmeier WW, Wilwerding TM. Effect of porcelain surface treatments on bond strengths of composite resin bonded to porcelain. J Prosthet Dent. 1994;72:355–359
  45. Shahverdi S, Canay S, Sahin E, Bilge A. Effects of different surface treatment methods on the bond strength of composite resin to porcelain. J Oral Rehabil. 1998;25:699–705
  46. Pameijer CH, Louw NP, Fischer D. Repairing fractured porcelain: how surface preparation affects shear force resistance. J Am Dent Assoc. 1996;127:203–209
  47. Szep S, Gerhardt T, Gockel HW, Ruppel M, Metzeltin D, Heidemann D. In vitro dentinal surface reaction of 9.5% buffered hydrofluoric acid in repair of ceramic restorations: a scanning electron microscopic investigation. J Prosthet Dent. 2000;83:668–674
  48. Lacy AM, LaLuz J, Watanabe LG, Dellinges M. Effect of porcelain surface treatment on the bond to composite. J Prosthet Dent. 1988;60:288–291
  49. Calamia JR. Etched porcelain veneers: the current state of the art. Quintessence Int. 1985;16:5–12
  50. Kern M, Thompson VP. Sandblasting and silica coating of a glass-infiltrated alumina ceramic: volume loss, morphology, and changes in the surface composition. J Prosthet Dent. 1994;71:453–461
  51. Kato H, Matsumura H, Atsuta M. Effect of etching and sandblasting on bond strength to sintered porcelain of unfilled resin. J Oral Rehabil. 2000;27:103–110
  52. Frankenberger R, Kramer N, Sindel J. Repair strength of etched vs silica-coated metal-ceramic and all-ceramic restorations. Oper Dent. 2000;25:209–215
  53. Kiatsirirote K, Northeast SE, van Noort R. Bonding procedures for intraoral repair of exposed metal with resin composite. J Adhes Dent. 1999;1:315–321
  54. Sun R, Suansuwan N, Kilpatrick N, Swain M. Characterization of tribochemically assisted bonding of composite resin to porcelain and metal. J Dent. 2000;28:441–445
  55. Horn HR. Porcelain laminate veneers bonded to etched enamel. Dent Clin North Am. 1983;27:671–684
  56. Bailey JH. Porcelain-to-composite bond strengths using four organosilane materials. J Prosthet Dent. 1989;61:174–177
  57. Bertolotti RL, Lacy AM, Watanabe LG. Adhesive monomers for porcelain repair. Int J Prosthodont. 1989;2:483–489
  58. Paffenbarger GC, Sweeney WT, Bowen RL. Bonding porcelain teeth to acrylic resin denture bases. J Am Dent Assoc. 1967;74:1018–1023
  59. Cooley RL, Tseng EY, Evans JG. Evaluation of 4-META porcelain repair system. J Esthet Dent. 1991;3:11–13
  60. Diaz-Arnold AM, Aquilino SA. An evaluation of the bond strengths of four organosilane materials in response to thermal stress. J Prosthet Dent. 1989;62:257–260
  61. Diaz-Arnold AM, Schneider RL, Aquilino SA. Bond strengths of intraoral porcelain repair materials. J Prosthet Dent. 1989;61:305–309
  62. Diaz-Arnold AM, Wistrom DW, Aquilino SA, Swift EJ. Bond strengths of porcelain repair adhesive systems. Am J Dent. 1993;6:291–294
  63. Llobell A, Nicholls JI, Kois JC, Daly CH. Fatigue life of porcelain repair systems. Int J Prosthodont. 1992;5:205–213
  64. Matsumura H, Kawahara M, Tanaka T, Atsuta M. A new porcelain repair system with a silane coupler, ferric chloride, and adhesive opaque system. J Dent Res. 1989;68:813–818
  65. Pratt RC, Burgess JO, Schwartz RS, Smith JH. Evaluation of bond strength of six porcelain repair systems. Dent Mat. 1992;8:158–161
  66. Stokes AN, Hod JA, Tidmarsh BG. Effect of 6-month water storage on silane-treated resin/porcelain bonds. J Dent. 1988;16:294–296
  67. Suliman AH, Swift EJ, Perdigao J. Effects of surface treatment and bonding agents on bond strength of composite resin to porcelain. J Prosthet Dent. 1993;70:118–120
  68. Aida M, Hayakawa T, Mizukawa K. Adhesion of composite to porcelain with various surface conditions. J Prosthet Dent. 1995;73:464–470
  69. Tjan AH, Nemetz H. A comparison of the shear bond strength between two composite resins and two etched ceramic materials. Int J Prosthodont. 1988;1:73–79
  70. Braga RR, Ballester RY, Carrilho MR. Pilot study on the early shear strength of porcelain-dentin bonding using dual-cure cements. J Prosthet Dent. 1999;81:285–289
  71. Soderholm KJ, Shang SW. Molecular orientation of silane at the surface of colloidal silica. J Dent Res. 1993;72:1050–1054
  72. Russell DA, Meiers JC. Shear bond strength of resin composite to Dicor treated with 4-META. Int J Prosthodont. 1994;7:7–12
  73. Chen TM, Brauer GM. Solvent effects on bonding organo-silane to silica surfaces. J Dent Res. 1982;61:1439–1443
  74. Barghi N, Chung K, Farshchian F, Berry T. Effects of the solvents on bond strength of resin bonded porcelain. J Oral Rehab. 1999;26:853–857
  75. Kramer N, Lohbauer U, Frankenberger R. Adhesive luting of indirect restorations. Am J Dent. 2000;13:60D–76D
  76. Blackman R, Barghi N, Duke E. Influence of ceramic thickness on the polymerization of light-cured resin cement. J Prosthet Dent. 1990;63:295–300
  77. Hasegawa EA, Boyer DB, Chan DC. Hardening of dual-cured cements under composite resin inlays. J Prosthet Dent. 1991;66:187–192
  78. el-Badrawy WA, el-Mowafy OM. Chemical versus dual curing of resin inlay cements. J Prosthet Dent. 1995;73:515–524
  79. Chang JC, Nguyen T, Duong JH, Ladd GD. Tensile bond strengths of dual-cured cements between a glass-ceramic and enamel. J Prosthet Dent. 1998;79:503–507
  80. Gregory WA, Moss SM. Effects of heterogeneous layers of composite and time on composite repair of porcelain. Oper Dent. 1990;15:18–22
  81. Hahn P, Attin T, Grofke M, Hellwig E. Influence of resin cement viscosity on microleakage of ceramic inlays. Dent Mater. 2001;17:191–196
  82. Frazier KB, Sarrett DC. Wear resistance of dual-cured rein luting agents. Am J Dent. 1995;8:161–164
  83. Kawai K, Isenberg BP, Leinfelder KF. Effect of gap dimension on composite resin cement wear. Quintessence Int. 1994;25:53–58
  84. Chung CH, Brendlinger EJ, Brendlinger DL, Bernal V, Mante FK. Shear bond strengths of two resin-modified glass ionomer cements to porcelain. Am J Orthod Dentofacial Orthop. 1999;115:533–535
  85. Berry T, Barghi N, Chung K. Effect of water storage on the silanization in porcelain repair strength. J Oral Rehabil. 1999;26:459–463
  86. Roulet JF, Soderholm KJ, Longmate J. Effects of treatment and storage conditions on ceramic/composite bond strength. J Dent Res. 1995;74:381–387
  87. Kato H, Matsumura H, Tanaka T, Atsuta M. Bond strength and durability of porcelain bonding systems. J Prosthet Dent. 1996;75:163–168
  88. Matsumura H, Kato H, Atsuta M. Shear bond strength to feldspathic porcelain of two luting cements in combination with three surface treatments. J Prosthet Dent. 1997;78:511–517
  89. Eikenberg S, Shurtleff J. Effect of hydration on bond strength of a silane-bonded composite to porcelain after seven months. Gen Dent. 1996;44:58–61
  90. Appeldoorn RE, Wilwerding TM, Barkmeier WW. Bond strength of composite resin to porcelain with newer generation porcelain repair systems. J Prosthet Dent. 1993;70:6–11
  91. Leibrock A, Degenhart M, Behr M, Rosentritt M, Handel G. In vitro study of the effect of thermo- and load-cycling on the bond strength of porcelain repair systems. J Oral Rehabil. 1999;26:130–137
  92. Øilo G. Bond strength testing—what does it mean?. Int Dent J. 1993;43:492–498
  93. Chadwick RG, Mason AG, Sharp W. Attempted evaluation of three porcelain repair systems—what are we really testing?. J Oral Rehabil. 1998;25:610–615
  94. Della Bona A, van Noort R. Shear vs. tensile bond strength of resin composite bonded to ceramic. J Dent Res. 1995;74:1591–1596
  95. McLean JW, Hughes TH. The reinforcement of dental porcelain with ceramic oxides. Br Dent J. 1965;119:251–267
  96. Seghi RR, Sorensen JA. Relative flexural strength of six new ceramic materials. Int J Prosthodont. 1995;8:239–246
  97. Andersson M, Oden A. A new all-ceramic crown: a dense-sintered, high-purity alumina coping with porcelain. Acta Odontol Scand. 1993;51:59–64
  98. Zeng K, Oden A, Rowcliffe D. Flexure tests on dental ceramics. Int J Prosthodont. 1996;9:434–439
  99. Zeng K, Oden A, Rowcliffe D. Evaluation of mechanical properties of dental ceramic core materials in combination with porcelains. Int J Prosthodont. 1998;11:183–189
  100. Ashizuka M, Kiyohara H, Okuno T, Kubota Y. Fatigue behavior of tetragonal zirconia polycrystals (Y-TZP) containing 2 and 4 mol% Y2O3 (Part 2). J Ceram Soc Jpn Inter Ed. 1988;96:731–736
  101. Taira M, Nomura Y, Wakasa K, Yamaki M, Matsui A. Studies on fracture toughness of dental ceramics. J Oral Rehabil. 1990;17:551–563
  102. Giordano RA, Pelletier L, Campbell S, Pober R. Flexural strength of an infused ceramic, glass ceramic, and feldspathic porcelain. J Prosthet Dent. 1995;73:411–418
  103. Kern M, Thompson VP. Bonding to glass infiltrated alumina ceramic: adhesive methods and their durability. J Prosthet Dent. 1995;73:240–249
  104. Sadoun M, Asmussen E. Bonding of resin cements to an aluminous ceramic: a new surface treatment. Dent Mater. 1994;10:185–189
  105. Kern M, Thompson VP. Sandblasting and silica-coating of dental alloys: volume loss, morphology and changes in the surface composition. Dent Mater. 1993;9:151–161
  106. Ozcan M, Alkumru HN, Gemalmaz D. The effect of surface treatment on the shear bond strength of luting cement to a glass-infiltrated alumina ceramic. Int J Prosthodont. 2001;14:335–339
  107. Isidor F, Stokholm R, Ravnholt G. Tensile bond strength of resin luting cement to glass infiltrated porous aluminium oxide cores (In-Ceram). Eur J Prosthodont Restor Dent. 1995;3:199–202
  108. Madani M, Chu FC, McDonald AV, Smales RJ. Effects of surface treatments on shear bond strengths between a resin cement and an alumina core. J Prosthet Dent. 2000;83:644–647
  109. Awliya W, Oden A, Yaman P, Dennison JP, Razzoog ME. Shear bond strength of a resin cement to densely sintered high-purity alumina with various surface conditions. Acta Odontol Scand. 1998;56:9–13
  110. Blixt M, Adamczak E, Linden LA, Oden A, Arvidson K. Bonding to densely sintered alumina surfaces: effect of sandblasting and silica coating on shear bond strength of luting cements. Int J Prosthodont. 2000;13:221–226
  111. Derand P, Derand T. Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont. 2000;13:131–135
  112. Kern M, Wegner SM. Bonding to zirconia ceramic: adhesion methods and their durability. Dent Mater. 1998;14:64–71
  113. Wegner SM, Kern M. Long-term resin bond strength to zirconia ceramic. J Adhes Dent. 2000;2:139–147
  114. Weinstein M, Katz S, Weinstein AB. Permanent Manufacturing Corporation, assignee. Fused Porcelain-to-Metal Teeth. U.S. Patent No. 3,052,982 September 11, 1962;
  115. McLaughlin G. Porcelain veneers. Dent Clin North Am. 1998;42:653–656 ix
  116. Culp L. Empress 2. First year clinical results. J Dent Technol. 1999;16:12–15
  117. Mackert J, Evans Al . Effect of cooling rate on leucite volume fraction in dental porcelains. J Dent Res. 1991;70:137–139
  118. McKinney JE, Wu W. Chemical softening and wear of dental composites. Dent Res. 1985;64:1326–1331
  119. Ortengren U, Andersson F, Elgh U, Terselius B, Karlsson S. Influence of pH and storage time on the sorption and solubility behaviour of three composite resin materials. J Dent. 2001;29:35–41
  120. Palmer DS, Barco MT, Billy EJ. Temperature extremes produced orally by hot and cold liquids. J Prosthet Dent. 1992;67:325–327
  121. Harrison A, Moores GE. Influence of abrasive particle size and contact stress on the wear rate of dental restorative materials. Dent Mater. 1985;1:14–18
  122. Paul SJ, Pietrobon N, Scharer P. The new In-Ceram Spinell system—a case report. Int J Periodontics Restorative Dent. 1995;15:520–527
  123. Piotrowski PR. Comparative studies on the adhesion of a silicone elastomer to a chromium-cobalt dental alloy. Eur J Prosthodont Restor Dent. 2001;9:141–146
  124. Wada T. Development of a new adhesive material and its properties. In:  Gettleman L,  Vrijhoef M,  Uchiyama Y editor. Proceedings of the international symposium on adhesive prosthodontics, 1986 June 24, Amsterdam, Netherlands. Chicago: Academy of Dental Materials; 1986;p. 9–18
  125. Tinschert J, Natt G, Mautsch W, Augthun M, Spiekermann H. Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study. Int J Prosthodont. 2001;14:231–238
  126. McLaren EA. All-ceramic alternatives to conventional metal-ceramic restorations. Compend Contin Educ Dent. 1998;19:307–308 310, 312
  127. Yildirim M, Edelhoff D, Hanisch O, Spiekermann H. Ceramic abutments—a new era in achieving optimal esthetics in implant dentistry. Int J Periodontics Restorative Dent. 2000;20:81–91
  128. Koutayas SO, Kern M. All-ceramic posts and cores: the state of the art. Quintessence Int. 1999;30:383–392
  129. Ahmad I. Zirconium oxide post and core system for the restoration of an endodontically treated incisor. Pract Periodontics Aesthet Dent. 1999;11:197–204
  130. Blatz MB. Comprehensive treatment of traumatic fracture and luxation injuries in the anterior permanent dentition. Pract Proced Aesthet Dent. 2001;13:273–279
  131. Fradeani M, Aquilano A, Barducci G. Aesthetic restoration of endodontically treated teeth. Pract Periodontics Aesthet Dent. 1999;11:761–768
  132. Meyenberg KH, Luthy H, Scharer P. Zirconia posts: a new all-ceramic concept for nonvital abutment teeth. J Esthet Dent. 1995;7:73–80
  133. Burke FJ. Fracture resistance of teeth restored with dentin-bonded crowns: the effect of increased tooth preparation. Quintessence Int. 1996;27:115–121

 Reprint requests to: Dr Markus B. Blatz, Louisiana State University Health Sciences Center, School of Dentistry, 1100 Florida Ave, New Orleans, LA 70119, Fax: (504) 619-8741, E-mail: mblatz@lsuhsc.edu

☆☆ aAssistant Professor, Department of Prosthodontics, Louisiana State University.

 bAssociate Professor, Department of Prosthodontics, Louisiana State University.

★★ cProfessor and Chairman, Department of Prosthodontics, Propaedeutics and Dental Materials, Christian Albrechts University Kiel.

 0022-3913/2003/$30.00 + 0

PII: S0022-3913(02)52750-5

doi: 10.1067/mpr.2003.50

Journal of Prosthetic Dentistry
Volume 89, Issue 3 , Pages 268-274 , March 2003